MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC ULTEM™ Resin 2410EPR Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Enhanced Electroplatability,Easy Flow,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant,Good Mold Release

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.56 g/cc1.56 g/ccASTM D792
Density 1.56 g/cc0.0564 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.400 %0.400 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.80 %0.80 %ISO 62-1
Viscosity 11 cP
@Load 5.00 kg,
Temperature 360 °C
11 cP
@Load 11.0 lb,
Temperature 680 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inSABIC method
 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0050 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 8.9 g/10 min
@Load 6.60 kg,
Temperature 337 °C
8.9 g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 165 MPa23900 psiH358/30; ISO 2039-1
Tensile Strength at Break 165 MPa23900 psi5 mm/min; ASTM D638
 170 MPa24700 psi5 mm/min; ISO 527
Tensile Strength, Yield 165 MPa23900 psi5 mm/min; ASTM D638
 170 MPa24700 psi5 mm/min; ISO 527
Elongation at Break 1.8 %1.8 %5 mm/min; ASTM D638
 2.0 %2.0 %5 mm/min; ISO 527
Elongation at Yield 1.8 %1.8 %5 mm/min; ASTM D638
 2.0 %2.0 %5 mm/min; ISO 527
Tensile Modulus 11.0 GPa1600 ksi1 mm/min; ISO 527
 11.1 GPa1610 ksi5 mm/min; ASTM D638
Flexural Strength 220 MPa31900 psiyield, 2 mm/min; ISO 178
 240 MPa34800 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.50 GPa1380 ksi2 mm/min; ISO 178
 10.65 GPa1545 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 82.0 J60.5 ft-lbASTM D256
Izod Impact, Unnotched 4.10 J/cm7.68 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²14.3 ft-lb/in²80*10*4; ISO 180/1U
 30.0 kJ/m²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 18.0 J13.3 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 120 - 180 sec120 - 180 secASTM D495
Comparative Tracking Index 100 - 175 V100 - 175 VUL 746A
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness >=0.400 mm
7.0 - 15 sec
@Thickness >=0.0157 in
UL 746A
 15 - 30 sec
@Thickness >=0.750 mm
15 - 30 sec
@Thickness >=0.0295 in
UL 746A
 60 - 120 sec
@Thickness >=1.50 mm
60 - 120 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=0.400 mm
0.00 - 15 arcs
@Thickness >=0.0157 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  15.0 µm/m-°C
@Temperature -40.0 - 150 °C
8.33 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
 15.0 µm/m-°C
@Temperature 23.0 - 150 °C
8.33 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow  45.0 µm/m-°C
@Temperature -40.0 - 150 °C
25.0 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
 45.0 µm/m-°C
@Temperature 23.0 - 150 °C
25.0 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 206 °C403 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 208 °C406 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 212 °C
@Thickness 3.20 mm
414 °F
@Thickness 0.126 in
unannealed; ASTM D648
 215 °C
@Thickness 6.40 mm
419 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 197 °C387 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 205 °C401 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 204 °C
@Thickness 3.20 mm
399 °F
@Thickness 0.126 in
unannealed; ASTM D648
 208 °C
@Thickness 6.40 mm
406 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 214 °C417 °FRate B/50; ISO 306
 215 °C419 °FRate B/120; ISO 306
 223 °C433 °FRate B/50; ASTM D1525
UL RTI, Electrical 105 °C221 °FUL 746B
UL RTI, Mechanical with Impact 105 °C221 °FUL 746B
UL RTI, Mechanical without Impact 105 °C221 °FUL 746B
Flammability, UL94 V-0
@Thickness >=0.400 mm
V-0
@Thickness >=0.0157 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 345 - 400 °C653 - 752 °F
Zone 2 340 - 400 °C644 - 752 °F
Zone 3 345 - 400 °C653 - 752 °F
Melt Temperature 350 - 400 °C662 - 752 °FInjection Molding
Mold Temperature 135 - 165 °C275 - 329 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 24.0 hour24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82634 / 290581

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.