MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® ABLESTIK 2332 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Black

Product Benefits:

  • One component
  • Excellent adhesion
  • Non-conductive
  • Low temperature cure
  • High strength
Cure: Heat cure

Application: Non-conductive adhesive

Surfaces: Copper, Aluminum, Nickel, FRP and Rigid plastics

LOCTITE ABLESTIK 2332 is a solventless epoxy adhesive that develops high bond strength when cured at temperatures as low as 100°C. This product combines toughness at low temperatures plus high peel and tensile shear strengths over a very broad temperature range.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 - 1.23 g/ccUncured
Viscosity 65000 - 85000 cPUncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 30
@Temperature 120 °C
Cured
 75
@Temperature 25.0 °C
Cured
Tensile Modulus 10.0 MPa
@Temperature 200 °C
Cured, DMTA
 20.0 MPa
@Temperature 150 °C
Cured, DMTA
 508 MPa
@Temperature 100 °C
Cured, DMTA
 1043 MPa
@Temperature 50.0 °C
Cured, DMTA
Shear Strength 1.20 MPa
@Temperature 50.0 °C
Lap, PBT, cured
 3.10 MPa
@Temperature 125 °C
Lap, PBT, cured
 4.90 MPa
@Temperature 150 °C
Lap, Aluminum, cured
 6.00 MPa
@Temperature 25.0 °C
Lap, PBT, cured
 12.5 MPa
@Temperature 125 °C
Lap, Aluminum, cured
 15.3 MPa
@Temperature 90.0 °C
Lap, Aluminum, cured
 20.4 MPa
@Temperature 25.0 °C
Lap, Aluminum, cured
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+14 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°CCured
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 105 °CCured, TMA
Shrinkage 2.3 %Cured
 
Processing PropertiesOriginal ValueComments
Cure Time 0.330 min
@Temperature 150 °C
Alternative Curing Conditions
 0.500 min
@Temperature 120 °C
Alternative Curing Conditions
 1.00 hour
@Temperature 120 °C
Typical
 1.50 min
@Temperature 100 °C
Alternative Curing Conditions
Shelf Life 6.00 Month
@Temperature 0.000 - 8.00 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5017 / 255228

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.