VESTAKEEP® 4000 G Black is a high viscosity, unreinforced PEEK for injection molding and extrusion. The semi-crystalline polymer features superior, thermal and chemical resistance. Parts made from VESTAKEEP® 4000 G are self-extinguishing. VESTAKEEP® 4000 G can be processed by common machines for thermoplastics. Property data for dry samples. Information provided by Evonik. |