MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Trimay® Wear Plate TWP57 Chromium-based Flux Cored Weld Wire & Electrode
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Description: TWP57 is a chromium-based flux cored wire electrode used to protect equipment and parts from heavy wear and mild-to-moderate direct impact. TWP57 has a compatible compostion that allows it to be applied on a wide array of materials and it maintains good Rockwell Hardness (HRc) and wear ability at elevated temperatures.

Key Performance Characteristics: Heavy abrasion and mild/moderate impact resistance, Compatible composition for welding, Hardness increase on underlying layer(s), Good hardness at elevated temperatures

Applications: TWP57 can be overlain on carbon steel, manganese base materials and mild or alloy steels. The maximum recomended deposit thickness of TWP56 is 2 - 3 layers, or 1/4” (6.35mm). TWP57 is used to cover exposed bolts and seams for installation of T156 wear plate and parts, as well as for small area lining of heavy wearing parts and equipment such as the front lip ‘bullnose’ of asphalt screeds.

Information provided by Trimay®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 59Wire, layer 1
 61 - 63Electrodes
 63Wire, layer 2
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 5.0 %
Chromium, Cr <= 30 %
Iron, Fe >= 62 %
Manganese, Mn <= 1.5 %
Silicon, Si <= 1.5 %
 
Descriptive Properties
Available Sizes: Electrode3.25[mm]
 4[mm]
 5[mm]
Available Sizes: Wire1.6[mm], cored wire
 2.4[mm], cored wire
 2.8[mm], cored wire
Packaging: Electrode3.5[mm] 4.5kg sleeves (4 sleeves=1 box)
 4[mm] 4.5kg sleeves (4 sleeves=1 box)
 5[mm] 5kg sleeves (4 sleeves=1 box)
Packaging: Wire1.6[mm], 25kg spools
 2.4[mm], 25kg spools
 2.8[mm], 25kg spools

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NTRIM007 / 120821

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.