MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Persian Gulf Polymer GPPS-1115 General Purpose Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: General Purpose Polystyrene (GPPS) 1115 with easy flow and good clarity. It is recommended for application where a specific balance of flow and strength are important. In injection, molding GPPS 1115 possesses low viscosity at high shear rate. It is particularly suitable for glossy-layer co extrusion. Application: Injection molding, disposable cups, pen barrels, crisper boxes for refrigerators, food containers, gloss layer co-extrusion, loose fill packaging and it can blend with HIPS.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption <= 0.090 %<= 0.090 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inASTM – D955
Melt Flow 9.0 - 11 g/10 min
@Load 5.00 kg,
Temperature 200 °C
9.0 - 11 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 42.0 MPa6090 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM – D638
Tensile Modulus 2.90 GPa421 ksiASTM – D638
Izod Impact, Notched (ISO) 1.50 kJ/m²0.714 ft-lb/in²ASTM D256
Izod Impact, Unnotched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 95.0 °C
@Load 1.02 kg
203 °F
@Load 2.25 lb
120°C/h; ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERSI912 / 250316

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.