MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ixom ALKATEQ™ XDS34P LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: ALKATEQ™ XDS34P is a natural, unpigmented, additive free, low density polyethylene ground powder with a typical particle size of 95% <500 micron. ALKATEQ™ XDS34P conforms to the requirements of the United States Food and Drug Administration Regulations CFR21 177.1520, paragraph (c), item 2.1. and, when used in accordance with FDA application guidelines, is suitable for food contact applications. Typical applications include abrasive additive in industrial cleansers and non slip coatings.

Information provided by Ixom Operations PTY LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.300 g/cc0.0108 lb/in³powder; ASTM D1895
Density 0.922 g/cc0.0333 lb/in³base polymer; ASTM D1505
Particle Size 150 µm150 µm<25%; ASTM D1921
 232 µm232 µm15-40%; ASTM D1921
 300 µm300 µm15-40%; ASTM D1921
 355 µm355 µm<25%; ASTM D1921
 425 µm425 µm<30%; ASTM D1921
 500 µm500 µm<5%; ASTM D1921
 710 µm710 µm<2%; ASTM D1921
 1180 µm1180 µm0; ASTM D1921
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PIXOM012 / 283093

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.