MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Goodfellow Multi Wall Graphene Nanotubes
Categories: Carbon

Material Notes: These nanotubes are functionalized using a split-plasma process, which does not damage the material as can be the case with acid treatment. Functionalization aids both dispersion and suspension in fluids such as epoxies, oils or composite matrices. These nanotubes are supplied dry, in a nano-suitable airtight container. The material can be supplied in the form of a kit comprising three levels of functionalization (low, medium and high) in individual pots, to allow customers to evaluate which level is the most suited for their application.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.30 g/cc0.0470 lb/in³
 
Descriptive Properties
Average Diameter9.5 nmTEM
Average Length1.5 µmTEM
FunctionalitiesCarbonyl [C=O] and Hydroxyl [OH]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® PB3060 60% Bronze, PTFE Filled Compound
Goodfellow Graphene Oxide (GO) Film
AGC Fluon® RB2515 15% Carbon Fiber, PTFE Filled Compound
AGC Fluon® PB3360T 60% Bronze, PTFE Filled Compound
AGC Fluon® PB2510 10% Carbon Fiber, PTFE Filled Compound

CGOODF099o / 239187

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.