Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.10 g/cc | 1.10 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 70 | 70 |
| 67 @Temperature 70.0 °C | 67 @Temperature 158 °F |
| 68 @Temperature 100 °C, Time 252000 sec | 68 @Temperature 212 °F, Time 70.0 hour |
| 70 @Temperature 23.0 °C, Time 252000 sec | 70 @Temperature 73.4 °F, Time 70.0 hour |
| 70 @Temperature 150 °C, Time 252000 sec | 70 @Temperature 302 °F, Time 70.0 hour |
| 70 @Temperature 70.0 °C, Time 252000 sec | 70 @Temperature 158 °F, Time 70.0 hour |
| 70 @Temperature 100 °C, Time 252000 sec | 70 @Temperature 212 °F, Time 70.0 hour |
| 71 @Temperature 125 °C, Time 252000 sec | 71 @Temperature 257 °F, Time 70.0 hour |
| 71 @Temperature 125 °C, Time 252000 sec | 71 @Temperature 257 °F, Time 70.0 hour |
| 73 @Temperature 150 °C, Time 252000 sec | 73 @Temperature 302 °F, Time 70.0 hour |
| 73 @Temperature 150 °C, Time 252000 sec | 73 @Temperature 302 °F, Time 70.0 hour |
Tensile Strength | 15.99 MPa | 2319 psi |
| 9.4493 MPa @Temperature 150 °C, Time 252000 sec | 1370.5 psi @Temperature 302 °F, Time 70.0 hour |
| 12.008 MPa @Temperature 23.0 °C, Time 252000 sec | 1741.6 psi @Temperature 73.4 °F, Time 70.0 hour |
| 15.653 MPa @Temperature 100 °C, Time 252000 sec | 2270.3 psi @Temperature 212 °F, Time 70.0 hour |
| 15.99 MPa @Temperature 150 °C, Time 252000 sec | 2319 psi @Temperature 302 °F, Time 70.0 hour |
| 15.99 MPa @Temperature 150 °C, Time 252000 sec | 2319 psi @Temperature 302 °F, Time 70.0 hour |
| 16.645 MPa @Temperature 100 °C, Time 252000 sec | 2414.1 psi @Temperature 212 °F, Time 70.0 hour |
| 16.660 MPa @Temperature 70.0 °C, Time 252000 sec | 2416.4 psi @Temperature 158 °F, Time 70.0 hour |
| 16.836 MPa @Temperature 125 °C, Time 252000 sec | 2441.9 psi @Temperature 257 °F, Time 70.0 hour |
| 16.836 MPa @Temperature 125 °C, Time 252000 sec | 2441.9 psi @Temperature 257 °F, Time 70.0 hour |
Elongation, Ultimate | 328 % | 328 % |
| 218.1 % @Temperature 150 °C, Time 252000 sec | 218.1 % @Temperature 302 °F, Time 70.0 hour |
| 275.8 % @Temperature 23.0 °C, Time 252000 sec | 275.8 % @Temperature 73.4 °F, Time 70.0 hour |
| 303.1 % @Temperature 100 °C, Time 252000 sec | 303.1 % @Temperature 212 °F, Time 70.0 hour |
| 328 % @Temperature 150 °C, Time 252000 sec | 328 % @Temperature 302 °F, Time 70.0 hour |
| 328 % @Temperature 150 °C, Time 252000 sec | 328 % @Temperature 302 °F, Time 70.0 hour |
| 333.9 % @Temperature 70.0 °C, Time 252000 sec | 333.9 % @Temperature 158 °F, Time 70.0 hour |
| 335.9 % @Temperature 100 °C, Time 252000 sec | 335.9 % @Temperature 212 °F, Time 70.0 hour |
| 349 % @Temperature 125 °C, Time 252000 sec | 349 % @Temperature 257 °F, Time 70.0 hour |
| 349 % @Temperature 125 °C, Time 252000 sec | 349 % @Temperature 257 °F, Time 70.0 hour |
100% Modulus | 2.38 MPa | 345 psi |
Tear Strength | 28.7 kN/m | 164 pli |
| 34.0 kN/m | 194 pli |
Compression Set | 8.9 % @Temperature 125 °C, Time 79200 sec | 8.9 % @Temperature 257 °F, Time 22.0 hour |
| 9.6 % @Temperature 100 °C, Time 79200 sec | 9.6 % @Temperature 212 °F, Time 22.0 hour |
| 11 % @Temperature 100 °C, Time 79200 sec | 11 % @Temperature 212 °F, Time 22.0 hour |
| 11.4 % @Temperature 150 °C, Time 79200 sec | 11.4 % @Temperature 302 °F, Time 22.0 hour |
| 11.4 % @Temperature 100 °C, Time 252000 sec | 11.4 % @Temperature 212 °F, Time 70.0 hour |
| 11.8 % @Temperature 70.0 °C, Time 79200 sec | 11.8 % @Temperature 158 °F, Time 22.0 hour |
| 12.1 % @Temperature 125 °C, Time 79200 sec | 12.1 % @Temperature 257 °F, Time 22.0 hour |
| 13.2 % @Temperature 150 °C, Time 79200 sec | 13.2 % @Temperature 302 °F, Time 22.0 hour |
| 13.2 % @Temperature 100 °C, Time 252000 sec | 13.2 % @Temperature 212 °F, Time 70.0 hour |
| 15.6 % @Temperature 70.0 °C, Time 79200 sec | 15.6 % @Temperature 158 °F, Time 22.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | <= -70.6 °C | <= -95.0 °F |
Shrinkage | 4.1 % @Temperature 70.0 °C | 4.1 % @Temperature 158 °F |
| 4.3 % @Temperature 70.0 °C | 4.3 % @Temperature 158 °F |
| -0.300 % @Temperature 150 °C, Time 252000 sec | -0.300 % @Temperature 302 °F, Time 70.0 hour |
| 0.00 % @Temperature 23.0 °C, Time 252000 sec | 0.00 % @Temperature 73.4 °F, Time 70.0 hour |
| 9.4 % @Temperature 100 °C, Time 252000 sec | 9.4 % @Temperature 212 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |
TR-10 Temperature | -51.1°C |