Pharmalene FL 35 PH is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion, extrusion & injection molding, manufactured using high pressure tubular technology. It is produced according to good manufacturing practices (GMP). Application: Pharmalene FL 35 PH is intended for the use within pharmaceutical sector and is characterized by good stretch ability and seal ability. Pharmalene FL 35 PH is suitable for the production of transdermal patches and other TTS applications or can be used for injection molded articles for healthcare applications. Film properties are typical of a blown film extruded at 200°C. Information provided by Versalis. |