MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
SABIC Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East)  (Unverified Data**)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: UV stabilized, non-FR PC/ABS of excellent flow and impact performance

This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D 792
Density 1.14 g/ccISO 1183
Moisture Absorption at Equilibrium 0.15 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.40 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 260 °C
[cm^3/10 min] Melt Volume Rate; ISO 1133
 25 g/10 min
@Load 5.00 kg,
Temperature 260 °C
[cm^3/10 min] Melt Volume Rate; ISO 1133
 28 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 53.0 MPa50 mm/min; ISO 527
 53.0 MPaType I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 54.0 MPa50 mm/min; ISO 527
 54.0 MPaType I, 50 mm/min; ASTM D 638
Elongation at Break 120 %50 mm/min; ISO 527
 120 %Type I, 50 mm/min; ASTM D 638
Elongation at Yield 4.5 %50 mm/min; ISO 527
 4.5 %Type I, 50 mm/min; ASTM D 638
Tensile Modulus 2250 MPa1 mm/min; ISO 527
 2300 MPa5 mm/min; ASTM D 638
Flexural Yield Strength 80.0 MPa2 mm/min; ISO 178
 89.0 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2200 MPa2 mm/min; ISO 178
 2300 MPa1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 400 J/m
@Temperature -30.0 °C
ASTM D 256
 590 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Notched (ISO) 30.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
 65.0 kJ/m²
@Temperature 23.0 °C
80*10*3; ISO 180/1A
Charpy Impact, Notched 30.0 kJ/m²
@Temperature -30.0 °C
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
 65.0 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 55.0 J
@Temperature 23.0 °C
ASTM D 3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 126 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 105 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 107 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Vicat Softening Point 126 °CRate B/50; ISO 306
 126 °CRate B/50; ASTM D 1525
 127 °CRate B/120; ISO 306
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Glow Wire Ignition Temperature 750 °C
@Thickness 3.00 mm
IEC 60695-2-13
 
Descriptive Properties
Ball Pressure Test, 75°C +/- 2°CPassIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABIC4857 / 118745

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.