Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwriters Laboratories UL 94 flammability classification of V-0 at 0.4 mm (0.016”) thick. Availability: - Asia Pacific
- Europe
- North America
Additive: Features:- Ductile
- Flame Retardant
- Good Crack Resistance
- Good Mold Release
- Good Toughness
- Halogenated
- High Elongation
- Ignition Resistant
- Low Density
- Lubricated
Uses:- Appliances
- Automotive Electronics
- Bobbins
- Connectors
- Electrical Housing
- Electrical Parts
- Electrical/Electronic Applications
- Fasteners
- Industrial Applications
- Lighting Applications
- Living Hinges
- Printed Circuit Boards
- Switches
Appearance: BlackForms: Pellets Processing Method: Injection Molding Information provided by Ascend Performance Materials. |