MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik 1C256 Seamless tube and pipe
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel

Material Notes: Sandvik 1C256 is a ferritic, heat resisting, stainless, chromium steel, characterized by:
  • good resistance to reducing sulphurous gases
  • good resistance to oxidation in air
  • This steel can be used at temperatures up to 850 °C (1560 °F). However, allowance should be made for the low creep strength at the highest temperatures in order to avoid distortion due to the inherent mass of the steel.

    Information provided by Sandvik

    EN 1.4724

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 7.70 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Vickers 196
    Tensile Strength, Ultimate 400 - 600 MPa
    Tensile Strength, Yield >= 250 MPa
    @Strain 0.2 %
    Elongation at Break >= 15 %
    Rupture Strength 1.00 MPa
    @Temperature 900 °C,
    Time 3.60e+8 sec
     1.90 MPa
    @Temperature 900 °C,
    Time 3.60e+7 sec
     2.30 MPa
    @Temperature 800 °C,
    Time 3.60e+8 sec
     4.30 MPa
    @Temperature 800 °C,
    Time 3.60e+7 sec
     5.00 MPa
    @Temperature 700 °C,
    Time 3.60e+8 sec
     9.50 MPa
    @Temperature 700 °C,
    Time 3.60e+7 sec
     20.0 MPa
    @Temperature 600 °C,
    Time 3.60e+8 sec
     35.0 MPa
    @Temperature 600 °C,
    Time 3.60e+7 sec
     55.0 MPa
    @Temperature 500 °C,
    Time 3.60e+8 sec
     100 MPa
    @Temperature 500 °C,
    Time 3.60e+7 sec
    Modulus of Elasticity 195 GPa
     120 GPa
    @Temperature 1000 °C
     125 GPa
    @Temperature 800 °C
     145 GPa
    @Temperature 600 °C
     180 GPa
    @Temperature 400 °C
     190 GPa
    @Temperature 200 °C
     
    Electrical PropertiesOriginal ValueComments
    Electrical Resistivity 0.0000750 ohm-cm
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 10.5 µm/m-°C
    @Temperature 20.0 - 100 °C
     11.5 µm/m-°C
    @Temperature 20.0 - 400 °C
     12.0 µm/m-°C
    @Temperature 20.0 - 600 °C
     12.5 µm/m-°C
    @Temperature 20.0 - 800 °C
     13.5 µm/m-°C
    @Temperature 20.0 - 1000 °C
    Specific Heat Capacity 0.500 J/g-°C
    @Temperature 20.0 °C
    Thermal Conductivity 21.0 W/m-K
    @Temperature 20.0 °C
     23.0 W/m-K
    @Temperature 500 °C
     
    Component Elements PropertiesOriginal ValueComments
    Aluminum, Al 1.0 %
    Carbon, C <= 0.040 %
    Chromium, Cr 12.5 %
    Iron, Fe 84.3 %As Balance
    Manganese, Mn 0.70 %
    Phosphorus, P <= 0.035 %
    Silicon, Si 1.0 %
    Sulfur, S <= 0.015 %
    Titanium, Ti 0.40 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Sandvik 1C356 Seamless tube and pipe
    AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
    Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy
    AISI 1050 Steel, cold drawn, low temperature, stress relieved, 50-75 mm (2-3 in) round
    Sandvik SAF 2205 Seamless tube and pipe

    NSANDV222 / 19116

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.