MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) KetaSpire® KT-880UFP Polyetheretherketone (PEEK)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: KetaSpire® KT-880UFP is the high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-colored, ultra-fine powder form. This ultra-fine PEEK powder is suitable for water borne coatings, electrostatically driven powder coatings, and resin pre-impregnation of continuous fiber composites. This ultra fine powder is produced to a median particle size D50 of about 10 micrometers.

KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent chemical resistance to acids, bases and a broad range of aggressive organic chemicals, best in class fatigue resistance, high thermal resistance, high purity and ease of melt processing.

These properties make KT-880UFP well-suited for applications in health care, transportation, electronics, chemical processing and other industrial uses.

The resin is also available in a natural-colored pellet form under the grade name KT-880 NT for injection molding applications.

Key Attributes: Chemical Resistant; Ductile; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; High Heat Resistance

Applications: Aerospace Applications; Automotive Applications; Electrical/Electronic Applications; Industrial Applications; Oil/Gas Applications

D50, median particle size by Microtrac Laser Diffraction, 7.5 to 12.5 microns.

Injection Notes: Back Pressure: minimum

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccASTM D792
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Viscosity 150 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
ASTM D3835
Melt Flow 36 g/10 min
@Load 2.16 kg,
Temperature 400 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 100 MPaASTM D638
Elongation at Break 10 - 20 %ASTM D638
Elongation at Yield 5.2 %ASTM D638
Tensile Modulus 3650 MPaASTM D638
Flexural Strength 153 MPaASTM D790
Flexural Modulus 3790 MPaASTM D790
Izod Impact, Notched 53.0 J/mASTM D256
Izod Impact, Unnotched NBASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
Melting Point 343 °C
Deflection Temperature at 1.8 MPa (264 psi) 160 °CUnannealed; ASTM D648
Glass Transition Temp, Tg 147 °CDSC
 
Descriptive Properties
Availability (as of March 2019)Africa & Middle East; Asia Pacific; Europe; Latin America; North America
ColorNatural Color
FormsPowder
ProcessingElectrostatic Spray Coating; Water-borne Coating

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y5246 / 238627

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.