MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Solef® PVDF AM Filament MSC NT 1
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Solef® PVDF AM Filament MSC NT 1 provides long term performance up to 120°C, including exceptional chemical resistance and outstanding UV, weathering and oxidation resistance. The product is also intrinsically endowed of a very high purity. These features make it particularly suited for outdoor applications, and applications in contact with harsh chemical environments, such as Chemical Processing Industry, Semiconductor Industry and Oil & Gas.

Applications: Additive Manufacturing (3D Printing); Industrial Applications; Oil/Gas Applications; Plumbing Parts

Features: Chemical Resistant; Flame Retardant; Good Weather Resistance; High Purity; Oxidation Resistant; UV Resistant

Printing conditions for data table:
- Filament drying conditions: drying not needed
- Extruder temperature: 225 - 235°C
- Bed temperature: 100°C
- Printing tool path: cross hatching in the XY plane

Test specimen parameters:
- Layer thickness: 0.2 mm
- 100% infill
- 3 shells
- Printing speed: 25 mm/s

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.72 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25.0 MPaASTM D638
Tensile Strength, Yield 30.0 MPaASTM D638
Elongation at Break 50 - 250 %ASTM D638
Elongation at Yield 10 %ASTM D638
Tensile Modulus 800 MPaASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 148 °C
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorWhite
FormsFilament
Processing3D Printing, Fused Filament Fabrication (FFF)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4492 / 280292

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.