MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ UFL36AS PPA (Global)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: LNP LUBRICOMP UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.58 g/ccASTM D792
Density 1.58 g/ccISO 1183
Water Absorption 0.30 - 0.40 %24hrs; ASTM D570
 0.30 - 0.40 %23°C/24hrs; ISO 62-1
Moisture Absorption 0.100 - 0.200 %50% RH, 24 hrs; ASTM D570
 0.100 - 0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cmSABIC method
Melt Flow 24 g/10 min
@Load 1.20 kg,
Temperature 340 °C
MVR [cc/10 min]; ISO 1133
 28 g/10 min
@Load 1.20 kg,
Temperature 340 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 188 MPa5 mm/min; ISO 527
 189 MPa5 mm/min; ASTM D638
Elongation at Break 1.7 %5 mm/min; ASTM D638
 2.3 %5 mm/min; ISO 527
Tensile Modulus 11200 MPa5 mm/min; ASTM D638
 11500 MPa1 mm/min; ISO 527
Flexural Strength 250 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 260 MPa2 mm/min; ISO 178
 71.0 MPa
@Temperature 200 °C
2 mm/min; ISO 178
 82.0 MPa
@Temperature 180 °C
2 mm/min; ISO 178
 97.0 MPa
@Temperature 150 °C
2 mm/min; ISO 178
 141 MPa
@Temperature 120 °C
2 mm/min; ISO 178
 194 MPa
@Temperature 100 °C
2 mm/min; ISO 178
 214 MPa
@Temperature 80.0 °C
2 mm/min; ISO 178
Flexural Modulus 9900 MPa1.3 mm/min, 50 mm span; ASTM D790
 10100 MPa2 mm/min; ISO 178
 3100 MPa
@Temperature 200 °C
2 mm/min; ISO 178
 3500 MPa
@Temperature 180 °C
2 mm/min; ISO 178
 3800 MPa
@Temperature 150 °C
2 mm/min; ISO 178
 5400 MPa
@Temperature 120 °C
2 mm/min; ISO 178
 7600 MPa
@Temperature 100 °C
2 mm/min; ISO 178
 8400 MPa
@Temperature 80.0 °C
2 mm/min; ISO 178
Flexural Strain at Break 2.8 %2 mm/min; ISO 178
 3.1 %
@Temperature 80.0 °C
2 mm/min; ISO 178
 3.9 %
@Temperature 100 °C
2 mm/min; ISO 178
 4.8 %
@Temperature 180 °C
2 mm/min; ISO 178
 4.8 %
@Temperature 200 °C
2 mm/min; ISO 178
 5.0 %
@Temperature 150 °C
2 mm/min; ISO 178
 5.3 %
@Temperature 120 °C
2 mm/min; ISO 178
Izod Impact, Notched 90.0 J/mASTM D256
Izod Impact, Unnotched 730 J/mASTM D4812
Izod Impact, Notched (ISO) 10.0 kJ/m²80*10*4; ISO 180/1A
 9.00 kJ/m²
@Temperature -40.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²80*10*4; ISO 180/1U
 45.0 kJ/m²
@Temperature -40.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 55.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 8.00 JASTM D3763
Coefficient of Friction, Dynamic 0.51ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.57ASTM D3702 Modified: Manual
K (wear) Factor 5.00 x 10-10 in³-min/ft-lb-hrWasher [10^-10 in^5-min/ft-lb-hr]; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
 22.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
 58.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Specific Heat Capacity 1.722 J/g-°CASTM E1269
Thermal Conductivity 0.240 W/m-KASTM D5930
Deflection Temperature at 0.46 MPa (66 psi) 293 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 275 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 283 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 258 °CRate B/120; ISO 306
 262 °CRate B/50; ASTM D1525
 262 °CRate B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Zone 1 310 - 320 °C
Zone 2 315 - 325 °CInjection Molding
Zone 3 325 - 340 °C
Melt Temperature 315 - 330 °CInjection Molding
Mold Temperature 150 - 170 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Moisture Content 0.15 %Injection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH92498 / 253622

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.