MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem Lowilite™ 55 UV Absorber
Categories: Other Engineering Material

Material Notes: Product Description: Lowilite™ 55 UV absorber is an ultraviolet light absorber belonging to the benzophenone class of UVAs.

Applications: Lowilite™ 55 UV absorber offers ultraviolet light protection to a wide range of polymers. It is strong absorber of ultraviolet radiation and has a high degree of photostability. Photochemical energy absorbed in the ultraviolet region is dissipated as thermal energy. High absorptivity combined with photostabilty and the ability to release absorbed energy make it as excellent stabilizer against the detrimental effect of ultraviolet light.

CAS No: 2440-22-4

EINECS: 219-470-5

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.650 - 0.950 g/cc
Molecular Weight 225 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 128 - 132 °C
Flash Point 205 °C
 
Descriptive Properties
AppearanceCrystal Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH541 / 315459

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.