MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ LUBRILOY™ Compound DX08333 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRILOY DX08333 compound is based on Polycarbonate (PC) resin containing proprietary lubricant and carbon fiber. Added features of this grade include: ESD Safe, PTFE-free Wear & Friction Solution and Balanced Mechanical Performance.

Features: Electrostatic discharge (ESD),Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.100 %0.100 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0035 cm/cm0.0035 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 72.0 MPa10400 psi5 mm/min; ASTM D638
 113 MPa16400 psi5 mm/min; ISO 527
Elongation at Break 2.2 %2.2 %5 mm/min; ASTM D638
 2.2 %2.2 %5 mm/min; ISO 527
Tensile Modulus 7.30 GPa1060 ksi5 mm/min; ASTM D638
 7.31 GPa1060 ksi1 mm/min; ISO 527
Flexural Strength 99.0 MPa14400 psiASTM D790
 113 MPa16400 psiISO 178
Flexural Modulus 6.10 GPa885 ksiASTM D790
 6.76 GPa980 ksi2 mm/min; ISO 178
Izod Impact Notched 60.0 J44.3 ft-lbASTM D256
Izod Impact, Unnotched 2.96 J/cm5.55 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 22.0 kJ/m²10.5 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 17.0 J12.5 ft-lbpeak; ASTM D3763
Impact Test 10.0 J7.38 ft-lbMultiaxial Impact; ISO 6603
K (wear) Factor 161 x 10-8 mm³/N-M80.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10 - 1.00e+6 ohm10 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
19.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 49.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
27.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 138 °C
@Thickness 3.20 mm
280 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 134 °C273 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 132 °C
@Thickness 3.20 mm
270 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81138 / 289085

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.