MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ITW Chockfast® Super Ceramic Repair Liquid Ceramic Filled Epoxy Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: SUPER CERAMIC Repair Liquid is a unique ceramic filled, high build, brush able epoxy coating. Formulated for unequaled chemical and corrosion resistance with outstanding wear properties under adverse environments.

USE & BENEFITS: SUPER CERAMIC Repair Liquid is ideally suited for liningand resurfacing all types of severe service equipment commonly found in chemical plants, power plants, pulp & paper mills, mining operations, water treatment plants and a variety of other industrial and marine applications.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
Flexural Strength 8000 psiASTM D790
Compressive Strength 16900 psiASTM D695
Adhesive Bond Strength 3125 psiAdhesive Tensile Shear; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 22.0 °C
approximate
Pot Life 15.0 min
@Temperature 22.2 °C
 
Descriptive Properties
Colorblackhardener
 dark orangehardener, after mixing
 orangeresin
Mix Ratio by volume5 to 1
Mix Ratio by weight10 to 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWC9028 / 239538

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.