Compound 19511 is a 50 durometer salmon colored general purpose Silicone elastomer. It exhibits good resistance to heat and compression set and will remain non brittle at very low temperatures. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 3 GE 504 A19 B37 EO16 EO36 F19 EA14 G11; 4 GE 507 A19 B37 EO16 EO36 F19 EA14; 5 GE 507 A19 B37 EO16 EO36 F19 EA14 ZZ-R-765 Class 2a & 2b Grade 50 A-A-59588 Class 2a & 2b Grade 50 AMS 3302 Information provided by Pressure Seals Inc. |