Low density / easy to occurs cleavage and produce the yellowing phenomenon by the ultraviolet light / it is obvious to produce the yellowing phenomenon which the non adding anti-yellowing agent of soft foam after exposing to ultraviolet light / with the good anti-yellowing property after adding the product.Information provided by Go Yen Chemical |