MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller ElastiSeal® WSS-2M Pumpable Sealer
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: ElastiSeal® WSS-2M is a butyl based, high viscosity, non-drying, pumpable sealer. It is used for automotive weatherstrips to prevent rust and to seal door, trunk, and liftgate flanges against air and moisture penetration.

Features and Benefits:

  • Seals and protects against corrosion
  • Will not harden or gel over time even at extreme temperatures
  • Excellent weathering characteristics
  • Excellent resistance to sag even at high temperatures
  • Easy, consistent application

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 90 %ASTM D2369
Ash <= 35 %
@Temperature 760 °C,
Time 3600 sec
ASTM D5630
Storage Temperature 4.00 - 38.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1.25 MPa
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
ColorCoarse / Black
ConsistencyThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL159 / 316950

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.