MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lord Adhesives 7610DTM Direct-to-metal Adhesive/Sealant
Categories: Polymer; Adhesive; Thermoset

Material Notes: LORD® 7610DTM direct-to-metal adhesive/sealant is a single-component, moisture-cure product offering excellent adhesion to various substrates including many plastics, glass, concrete, wood and metals, especially precoated metals.

Features: creates high strength bonds, replacing mechanical fastening methods; exhibits excellent primerless adhesive properties. requires no mixing; cures quickly even at low temperatures; requires no ovens or other heat sources for curing. solvent resistant when cured. Painting and most cleaning processes do not affect bond strength. remains in position when applied on vertical or overhead surfaces, allowing for greater process flexibility. uncured material can endure 255°F (107°C) for 60 minutes, and cured material can endure 325°F (163°C) for 60 minutes with no negative effect. resists weathering and aging; provides excellent resistance to indirect UV exposure. low VOC content; contains no solvent.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50
Tensile Strength >= 200 psi
Elongation at Break >= 400 %ASTM D412
Shear Strength 200 - 500 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 325 °F
 
Processing PropertiesOriginal ValueComments
Pot Life 6.00 - 12.0 min
@Temperature 25.0 °C
Time to Handling Strength
Working Life 25.0 - 35.0 min
@Temperature 25.0 °C
work time, 50% RH
 
Descriptive Properties
AppearanceWhite, Black or Grey Paste
Processing Time15-45Skin Time, 25 C, 50% RH
 Immediately and up to 30 days without a scuffPaint Time

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Thermal Ceramics Therm-O-Stix Fibrous Adhesive
Overview of materials for Methacrylate Adhesive
Overview of materials for Epoxy Adhesive
Momentive Performance Materials RTV6809 Aluminum Adhesive Sealant, Industrial Plastic Adhesive
Momentive Performance Materials RTV109 Aluminum Adhesive Sealant, High Strength Paste

PLORD9140 / 232528

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.