MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Copper Alloy, UNS C64750, TF00 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Precipitation Hardened

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.91 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 190
@Load 3.00 kg
190
@Load 6.62 lb
Tensile Strength 614 MPa89000 psi
Tensile Strength, Yield 565 MPa82000 psi0.2% Offset
Elongation at Break 7.0 %7.0 %
Tensile Modulus 135.0 GPa19580 ksi
Shear Strength 265 MPa38400 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000380 ohm-cm0.00000380 ohm-cm45% IACS
Magnetic Permeability 1.01.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 100 °C
9.00 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Melting Point 1055 - 1078 °C1931 - 1972 °F
Solidus 1055 °C1931 °F
Liquidus 1078 °C1972 °F
Annealing Point >= 700.0 °C>= 1292 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 550.0 °C>= 1022 °FStress Relief
Solution Temperature >= 750.0 °C>= 1382 °F
Hot-Working Temperature >= 950.0 °C>= 1742 °F
Precipitation Temperature >= 450 °C>= 842 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 93.2 - 98.9 %93.2 - 98.9 %As Balance
Iron, Fe <= 1.0 %<= 1.0 %
Magnesium, Mg <= 0.10 %<= 0.10 %
Nickel, Ni 1.0 - 3.0 %1.0 - 3.0 %
Phosphorus, P <= 0.10 %<= 0.10 %
Silicon, Si 0.10 - 0.70 %0.10 - 0.70 %
Tin, Sn 0.050 - 0.80 %0.050 - 0.80 %
Zinc, Zn <= 1.0 %<= 1.0 %
Zirconium, Zr <= 0.10 %<= 0.10 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC64750x1 / 292232

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.