MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP93FRHT Two component epoxy system
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Twelve second vertical burn per AITM 2.0002B and Section 7.1.2 of ABD0031, Issue F
  • Smoke emission per AITM 2.0007B, Issue 3 in the flaming mode and Section 7.3.2 of ABD0031, Issue F
  • Toxic gas emission per AITM 3.0005, Issue 2 in the flaming mode and Section 7.4 of ABD0031, Issue F
Master Bond EP93FRHT is a two component epoxy that meets Airbus specifications. It can be employed as an adhesive, sealant and encapsulating system. It is used in all kinds of aircraft where protection is needed from flames, smoke and materials that might burn. It is most likely to be used in interior panels, floor and door assemblies, as well as frame lining. It also can be used for potting electronics. EP93FRHT is a non-halogenated type of flame retardant epoxy. This epoxy is a moderate viscosity system with a very long open time. It has an easy to use one to one mix ratio by weight. The recommended cure for optimizing properties is overnight at room temperature followed by 3-5 hours at 150-200°F. It bonds well to a variety of substrates including metals, composites, glass, ceramic and many plastics. The service temperature range is -80°F to +400°F. One particularly outstanding feature of this system after curing is its ability to withstand rigorous thermal cycling. It has good chemical resistance to water, fuels, oils and many common solvents. The color of Part A is black, Part B is off white and the cured material is dark gray. Since this system is color coded, it makes mixing more user friendly. EP93FRHT is a specialty product primarily for aviation and avionic applications where the demanding Airbus requirements for the vertical burn test, smoke emission and toxic gas emission as noted above are needed.

Product Advantages:

  • One to one mix ratio by weight and color coded
  • Excellent electrical insulator
  • Top notch adhesion to a wide variety of substrates
  • Low shrinkage upon curing
  • Passes the stringent requirements of the Airbus specifications mentioned above
  • Non halogen filler

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 1000 - 4000 cPPart B
 6000 - 9000 cPmixed
 80000 - 120000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80 - 90
Tensile Strength 4000 - 5000 psi
Elongation at Break 5.0 - 10 %
Tensile Modulus 250000 - 300000 psi
Adhesive Bond Strength 1200 - 1400 psilap shear, Al/Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.5
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 - 45.0 µm/m-°C
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -80.0 °F
 
Processing PropertiesOriginal ValueComments
Working Life 120 - 180 minAfter mixing, 100 g batch
Shelf Life 6.00 MonthIn original unopened containers
 
Descriptive Properties
Cure scheduleovernight at room temperature followed by 3-5 hours at 150-200°F
Mixing Ratio1:1Parts A to B, by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® FST2 Thermoplastic

PMASTM722 / 233779

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.