Compound 3418 is a 40 durometer black colored Buna N elastomer, it is formulated with Teflon to provide internal lubrication. It exhibits good low temperature flexibility. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BG 410 B14 B34 EA14 EO34 F17; 5 BG 410 A14 B14 B34 EO34 Information provided by Pressure Seals Inc. |