MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Melos Mecoline IS RDX 1207 F Halogen-free, radiation cross-linkable, flame retardant insulation and sheathing
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, radiation cross-linkable, flame retardant insulation and sheathing compound for photovoltaic/solar cables

Compound class: Sheathing

Compound category: RDX

Flame retardant: ATH

Standards: DIN/VDE DKE AK 411.2.3; TUV 2 PfG 1169/08.2007

Typical applications: Halogen-free, low smoke, UV and ozone resistant, max. operating temperature 125°C, radiation cross-linkable, flame retardant compound for photovoltaic/solar cables for Green Energy/Solar applications.

Features: Flame retardant; Halogen-free; Low smoke; High temperature resistant

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccpressed plaques, 155°C / 5 min.; DIN EN ISO 1183-1A
pH >= 4.5Corrosivity; IEC 60754-2
Melt Flow 27 g/10 min
@Load 21.6 kg,
Temperature 170 °C
DIN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 49pressed plaques, 155°C / 5 min.; DIN ISO 7619-1
Tensile Strength 10.0 MPaextruded tapes; IEC 60811-501
 12.3 MPacross-linked plaques or tapes, 175kGy; IEC 60811-501
Elongation at Break >= 30 %at break at -40°C; IEC 60811-501
 160 %cross-linked plaques or tapes, 175kGy; IEC 60811-501
 225 %extruded tapes; IEC 60811-501
 5.0 %
@Temperature 200 °C,
Time 900 sec
Hot set test, Residual, 0.2 Mpa (175kGy); IEC 60811-507
 13 %
@Temperature 250 °C,
Time 900 sec
Hot set test, Residual, 0.2 Mpa (175kGy); IEC 60811-507
 15 %
@Temperature 200 °C,
Time 900 sec
Hot set test, under load, 0.2 Mpa (175kGy); IEC 60811-507
 60 %
@Temperature 250 °C,
Time 900 sec
Hot set test, under load, 0.2 Mpa (175kGy); IEC 60811-507
Penetration 24
@Temperature 140 °C,
Time 14400 sec
IEC 60811-508
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+11 ohm-cm
@Temperature 90.0 °C
500V; EN 50395
 >= 1.00e+14 ohm-cm
@Temperature 20.0 °C
500V; EN 50395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 180 °CMaximum mass temperature
 170 - 190 °CTool
Zone 1 130 - 150 °C
Zone 2 140 - 160 °C
Zone 3 150 - 170 °C
Zone 4 160 - 180 °C
Zone 5 160 - 180 °C
Adapter Temperature 165 - 185 °C
Head Temperature 170 - 190 °C
Drying Temperature 60.0 - 70.0 °C
Dry Time 4.00 - 6.00 hour
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 34 %pressed plaques, 155°C / 5 min.; ASTM D 2863 A
 
Descriptive Properties
Cold bend testPassat -40°C, IEC 60811-506
Conductivity=10 µS/mmpressed plaques, 155°C / 5 min, IEC 60754-2
Impact strengthPassat -15°C, IEC 60811-506
Temperature index250°CASTM D 2863 D

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMELOS023 / 296130

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.