MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Huber MoldX® P12 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: MoldX® P12 is a non-halogen, optimized ATH product designed for fiberglass reinforced polyester applications such as pultrusion, resin infusion and vacuum bag molding. These molding processes have increased capability when used with MoldX® P12. MoldX® P12 has a narrow particle size distribution that has a small particle top size. This allows all the ATH particles to flow readily throughout the fiberglass reinforcement. An optimized particle size distribution with a small particle top size is a major advance for pultrusion. The pultruder can obtain a very low pull force at high glass content (> 50% by weight) especially when compared to other standard ATH products. MoldX® P12 allows formulators to pass stringent certification tests such as ASTM E84 Class A without the use of halogenated flame retardants such as Deca-BDE. Technical service is available.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.42 g/cc
Bulk Density 0.450 g/ccloose
 0.880 g/ccpacked
Brightness 95 %TAPPI
Moisture Absorption 0.250 %
@Temperature 105 °C
Free
Particle Size >= 4.5 µmMedian Particle Diameter
 <= 12 µm>99 percent
Particle Mesh Size 325 Mesh0.01% on
 325 Mesh99.99% through
Specific Surface Area 4.2 m²/gBET
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 0.0070 %
Loss on Ignition(%) 34.6 %
@Temperature 1000 °C
Na2O 0.025 %soluble
 2.0 %total
SiO2 0.0050 %
 
Descriptive Properties
Al(OH)3 (%)99.6
FunctionalityHigh Filler Loading Levels
 Smoke Suppression
Market/Application: ThermoplasticsPultrusion
Market/Application: ThermosetsWet Mat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EHUBER754 / 300860

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.