MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Saint-Gobain CHR® K350 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Tape; Thermoset; Polyimide, TS; Silicone

Material Notes: CHR® K350 is manufactured from polyimide film with high-temperature adhesive.

Features/Benefits: CHR® K350 has excellent mechanical and electrical properties as well as a high conformability. CHR® K350 offers outstanding resistance to cut through and are impact and abrasion resistant. They also offer excellent dielectric strength, while the burning of the adhesive forms a non-conductive ash. CHR® K350 meets the Underwriters Laboratories, Inc. Guide OANZ2 and File E51201 and File E66639 specifications respectively with a 180°C temperature rating, and it complies with UL510 for a flame retardant. Acrylic adhesive can be thermoset. The polyimide backing meets MIL-P-46112B.

Applications: CHR® K350 is constructed to fill the requirements of a high performance thermoplastic polyimide backing materials. CHR® K350 is designed to fill the various needs of electrical insulation requirements.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 75 %
Tear Strength 50.0 pliInitial Tear Strength
Peel Strength 0.220 kN/mAdhesion to Steel
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 10000 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -100 °F
 
Descriptive Properties
ColorAmber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger TECASINT 3012 Polyimide, Ochre Brown (PI)
Ensinger Sintimid™ V 15% graphite Polyimide (PI)
DuPont™ Kapton® 50FPC Polyimide Film, 13 Micron Thickness
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness
DuPont™ Cirlex® Polyimide Laminate

PSTGQZ333 / 68847

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.