MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Machined Parts
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: Higher abrasion resistance than G15, high value stability and very low friction coefficient property

Information provided by Daelim H&L

Key Words: PI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.63 g/cc1.63 g/ccASTM D792
Moisture Absorption at Equilibrium 0.85 %0.85 %50% RH; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 68 - 7868 - 78ASTM D785
Tensile Strength, Ultimate  41.1 MPa
@Temperature 260 °C
5960 psi
@Temperature 500 °F
ASTM D1708
 73.2 MPa
@Temperature 23.0 °C
10600 psi
@Temperature 73.4 °F
ASTM D1708
Tensile Strength, Yield 32.6 MPa
@Strain 1 %
4720 psi
@Strain 1 %
ASTM D95
Tensile Stress at Strain 115 MPa
@Strain 10 %
16600 psi
@Strain 10 %
ASTM D95
Elongation at Break  5.7 %
@Temperature 260 °C
5.7 %
@Temperature 500 °F
ASTM D1708
 6.5 %
@Temperature 23.0 °C
6.5 %
@Temperature 73.4 °F
ASTM D1708
Flexural Strength  48.1 MPa
@Temperature 260 °C
6980 psi
@Temperature 500 °F
ASTM D790
 90.4 MPa
@Temperature 23.0 °C
13100 psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus  2.76 GPa
@Temperature 260 °C
400 ksi
@Temperature 500 °F
ASTM D790
 4.848 GPa
@Temperature 23.0 °C
703.2 ksi
@Temperature 73.4 °F
ASTM D790
Compressive Modulus 3.3864 GPa
@Temperature 23.0 °C
491.16 ksi
@Temperature 73.4 °F
ASTM D695
Izod Impact, Notched (ISO) 4.3164 kJ/m²2.0543 ft-lb/in²ASTM D256
Coefficient of Friction 0.140.14
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 ohm-cm - 1e+05
@Temperature 23.0 °C
10000 ohm-cm - 1e+05
@Temperature 73.4 °F
ASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.40 µm/m-°C
@Temperature 23.0 - 260 °C
1.89 µin/in-°F
@Temperature 73.4 - 500 °F
ASTM D696
Decomposition Temperature 616 °C1140 °F
Oxygen Index 53.7 %53.7 %ASTM D2863
 
Descriptive Properties
50% Weight Reduction Time (Minutes)240

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Machined Parts
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Machined Parts
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Tubes
Ensinger TECASINT 1101 Polyimide (PI)
Daelim H&L Plavis MS Aromatic Polyimide, 15% MoS2 Filled, Machined Parts

PDAEL005 / 82659

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.