MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ AM Compound ZF004XXAR1 Polyphenylene Ether + PPS (PPE+PPS)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Sulfide (PPS)

Material Notes: LNP THERMOCOMP ZF004XXAR1 compound is based on Polyphenylene Ether / Polystyrene (PPE/PS) blend containing 20% glass fiber for Large Format Additive Manufacturing (LFAM) applications. Added features of this grade include: Lower Thermal Expansion, Improved Hydrolytic Stability, Higher Strength to Weight Ratio and Higher Temperature Performance vs. ABS.

Features: Hydrolytic Stability,High Heat Resistance,Good dimensional stability

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Moisture Absorption 0.0200 %Extrusion
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 28.0 MPa5mm/min; ASTM D638 Modified
 68.0 MPa5mm/min; ASTM D638 Modified
Elongation at Yield 1.9 %5 mm/min; ZX Orientation; ASTM D638 Modified
 2.0 %5 mm/min; XZ Orientation; ASTM D638 Modified
Tensile Modulus 2.70 MPa5 mm/min; ZX Orientation; ASTM D638 Modified
 5.20 MPa5 mm/min; XZ Orientation; ASTM D638 Modified
Flexural Strength 51.0 MPa5 mm/min; ASTM D790 Modified
 103 MPa5 mm/min; ASTM D790 Modified
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 131 °C
@Thickness 3.20 mm
annealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 100 - 120 °CBed Temperature
Nozzle Temperature 280 - 320 °C
Zone 1 270 - 305 °CExtrusion
Zone 2 280 - 320 °CExtrusion
Zone 3 280 - 320 °CExtrusion
Zone 4 280 - 320 °CExtrusion
Melt Temperature 270 - 305 °CExtrusion
Drying Temperature 120 °CExtrusion
Dry Time 4.00 hourExtrusion
Hold Pressure <= 13.5 MPaExtruder Pressure
 
Descriptive Properties
Extruder L/D24

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82502 / 290449

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.