MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Marco Polo MARPOL HDP PE100 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Description: MARPOL® HDP PE100 is a bimodal polyethylene resin to be used for pipe applications where long-term hydrostatic strength combined with outstanding resistance to slow crack growth, rapid crack propagation, chlorinated water and high melt strength is needed. This resin has excellent processability for the full range of pipe sizes and wall thicknesses to include heavy wall pipe.

Recommended Applications: Natural gas distribution pipes, large diameter industrial piping, mining, sewage and municipal water service lines

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.949 g/cc0.0343 lb/in³Natural; ASTM D792
 0.959 g/cc0.0346 lb/in³Black; ASTM D792
Melt Flow  0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 13 g/10 min
@Load 21.6 kg,
Temperature 190 °C
13 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT 10000 hour
@Temperature 80.0 °C
10000 hour
@Temperature 176 °F
Slow Crack Growth; ASTM F1473
Tensile Strength at Break >= 32.1 MPa>= 4660 psiASTM D638
Tensile Strength, Yield >= 24.1 MPa>= 3500 psiASTM D638
Elongation at Break 500 %500 %ASTM D638
Elongation at Yield 16 %16 %ASTM D638
Flexural Modulus 0.924 GPa134 ksiASTM D790B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 127 °C261 °FASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO200 / 283797

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.