MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman Premi-Glas® 2103-10 CRSX Polyester BMC
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:
  • Underwriters Laboratories, U.L. 94-V0 flame recognition at 2.54mm minimum wall thickness.
  • U.L. recognized in all colors.
  • Available in glass contents ranging from 10% - 30%; standard product has 22% reinforcement.
  • Excellent dielectric strength, arc and track resistance.
  • Chemical resistant and self-extinguishing properties.
  • Designed for Compression, Transfer and Injection molding processes

Data provided by Premix.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 - 1.85 g/cc
Linear Mold Shrinkage 0.0015 - 0.0035 cm/cmPolymerization Shrinkage
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 33.0 MPaASTM D638
Tensile Modulus 12.0 GPaASTM D638
Flexural Strength 95.0 MPaASTM D790
Flexural Modulus 9.70 GPaASTM D790
Poissons Ratio 0.30
Shear Modulus 4.60 GPaCalculated
Izod Impact, Notched 185 J/mASTM D256
Izod Impact, Unnotched 3.20 J/cmASTM D4812
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 15.0 kV/mmASTM D149
Arc Resistance 180 secASTM D495
Comparative Tracking Index 600 VASTM D2303
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°CZ Direction
CTE, linear, Transverse to Flow 25.0 µm/m-°CXY Direction
Thermal Conductivity 0.300 W/m-K
UL RTI, Electrical 130 °CUL 746C
UL RTI, Mechanical with Impact 130 °CUL 746C
UL RTI, Mechanical without Impact 130 °CUL 746C
Flammability, UL94 V-0
@Thickness 2.50 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 °CCompression or Injection Molding
Clamp Pressure 500 - 1000 psiMolding Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® UP 804 Unsaturated Polyester Resin, High Surface Quality, UL Listed, Low Shrinkage, High Arc Resistance
A. Schulman Premi-Glas® 3101-25 Polyester BMC
A. Schulman BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
A. Schulman BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
A. Schulman BMC 200 Thermoset Polyester, Electrical Grade

PPREMIX66 / 58202

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.