MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Syensqo (Solvay Specialty Polymers) KetaSpire® CF10 HC AM Filament PEEK, 10% carbon fiber
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Ketaspire® CF10 HC AM Filament incorporates 10% carbon fiber reinforcement into a PEEK matrix for increased strength offered for use in high-performance healthcare applications. This material provides long-term performance up to 240 °C, including exceptional chemical resistance. These properties make it particularly suited for metal replacement.

Applications: Medical Devices; Medical/Healthcare Applications

Features: Biocompatible; Chemical Resistant; Ductile; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; High Heat Resistance; High Strength

Printing conditions for data table:
- Filament drying conditions, minimum 4h: 150°C
- Extruder temperature: 400-440°C
- Bed temperature: 180-220°C
- Printing tool path: 0°

Test specimen parameters:
- First layer: 0.3mm thick
- Subsequent layers: 0.1mm
- 100% infill
- 3 shells
- Printing speed: 18 mm/s

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 140 MPa20300 psiASTM D638
Elongation at Break 1.7 %1.7 %ASTM D638
Tensile Modulus 11.0 GPa1600 ksiASTM D638
Izod Impact, Notched 0.890 J/cm1.67 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C649 °F
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
Diameter1.75 mm
FormsFilament
Processing3D Printing, Fused Filament Fabrication (FFF)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4310 / 280110

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.