General Description ER-MITE powders and dispersions are inorganic erbium-oxide nanoparticles. ER-MITE-A products are uncoated and hydrophilic. ER-MITE-O products are coated with an organic silane (1-4%) and are hydrophobic. Particles are available in the size range of 10-200 nm. |
Formula: Er2O3; CAS Number: 12061-16-4 |