MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
HB Fuller Cyberbond CB 2999 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive

Material Notes: Neomer Series: fast bonding; very high viscosity and surface insensitive. The Neomer Series stands for the so called surface in sensitive Cyanoacrylates. These products perform very well on most materials including acid surfaces such as wood, leather, cardboard, paper etc. CB 2999 is a thixotrpoic product or also called Gel, meaning that once applied the adhesive will stand even on vertical surfaces. In addition it has got very good gap filling properties.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/cc
Viscosity 3000 - 6000 cPcone-plate, 160 rpm @ 20 °C
 35000 - 60000 cPcone-plate, 0.5 rpm @ 20 °C
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 725 - 1740 psiNBR-rubber
 1160 - 2470 psisteel
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 95.0 °C
Minimum Service Temperature, Air -55.0 °C
Flash Point 80.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 10.0 secSet time, EPDM
 13.0 - 15.0 secSet time, plastic (ABS)
 45.0 - 120 secSet time, metal (Steel)
 80.0 - 120 secSet time, wood (beech)
Shelf Life 12.0 Month
 
Descriptive Properties
Base compoundEthyl-2-cyanoacrylate
Colorcolourless, transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL029 / 316820

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.