MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ascend Performance Materials Starflam® P10003 PA6 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Starflam P10003 is a mineral filled, flame retardant PA6 for injection molded applications. The material is halogen free and red phosphorus free.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³DAM; ISO 1183
Water Absorption 0.90 %
@Time 86400 sec
0.90 %
@Time 24.0 hour
DAM; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 71.0 MPa10300 psiDAM; ISO 527-2
Elongation at Break 2.7 %2.7 %DAM; ISO 527-2
Tensile Modulus 6.70 GPa972 ksiDAM; ISO 527-2
Flexural Strength 122 MPa17700 psiDAM; ISO 178
Flexural Modulus 6.20 GPa899 ksiDAM; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 179 °C354 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °FUnannealed; DAM; ISO 75-2/A
Flammability, UL94 V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 245 - 255 °C473 - 491 °FInjection
Middle Barrel Temperature 250 - 260 °C482 - 500 °FInjection
Front Barrel Temperature 250 - 260 °C482 - 500 °FInjection
Melt Temperature 255 - 265 °C491 - 509 °FInjection
Mold Temperature 55.0 - 95.0 °C131 - 203 °FInjection
Drying Temperature 75.0 - 85.0 °C167 - 185 °FInjection
Dry Time 4.00 hour4.00 hourInjection
Moisture Content 0.20 %0.20 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
Agency RatingsISO, 1043 PA6 FR(61)
AppearanceNatural Color
FeaturesFlame Retardant
 Good Electrical Properties
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8507 / 296294

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.