MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC FPC70 PP (Global)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: As part of SABIC® PP FLOWPACT portfolio, FPC70 delivers high top load performance (potential downgauging) with a superior stiffness / impact balance. It is nucleated and has good antistatic performance with easy demoulding. This grade has good flow behavior, and it was designed for high-speed injection moulding process, potentially enabling very cost efficient processing on the basis of easy mould filling and very short cycle times. Applications: SABIC® PP FPC70 is typically used in rigid packaging applications for both food and non-food industries. This includes packaging for yellow fats, cheese spreads, dairy, frozen, chilled and ambient food, household chemicals and paints among others. It can be also used in several applications in the caps & closures as well in housewares. The grade has excellent heat deflection temperature making it particularly suitable for hot fill applications. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by Sabic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 70 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 28.0 MPaISO 527-2 1A
Elongation at Yield 4.0 %ISO 527-2 1A
Tensile Modulus 1700 MPaISO 527-2 1A
Izod Impact, Notched (ISO) 6.00 kJ/m²ISO 180/1A
 3.00 kJ/m²
@Temperature -20.0 °C
ISO 180/1A
 4.00 kJ/m²
@Temperature 0.000 °C
ISO 180/1A
Charpy Impact, Notched 7.00 kJ/m²ISO 179/1eA
 3.00 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 5.00 kJ/m²
@Temperature 0.000 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CISO 75
Vicat Softening Point 80.0 °Cat 50 N (VST/B); ISO 306
 150 °Cat 10 N (VST/A); ISO 306
 
Descriptive Properties
Anti static agentTrue
Nucleating agentTrue

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Pro-fax SD242 Polypropylene Impact Copolymer
Braskem CP 404XP HECO Polypropylene Heterophasic Copolymer
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications

PSABI31248 / 229272

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.