MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Teknor Apex Medalist® MD-12180 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-12100 Series are high performance thermoplastic elastomer designed for use in healthcare and medical applications requiring high elasticity and excellent moldability. Medalist MD-12180 is a higher hardness, low density, translucent grade, available in NAT and colors, which can be sterilizable and exhibits excellent adhesion to polypropylene.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Moldability; Good Sterilizable; Good Toughness; Halogen Free; Low Density; Medium Flow; High Hardness; Low Specific Gravity; Lubricated; Radiation Sterilizable; Resilient; Slip; Without Fillers

Uses: Bushings; Closures; Disposable Hospital Goods; Flexible Grips; Grommets; Knobs; Medical/Healthcare Applications; Pharmaceuticals; Plugs; Rubber Replacement

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data.

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.893 g/cc0.0323 lb/in³ASTM D792
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  80
@Time 5.00 sec
80
@Time 0.00139 hour
ASTM D2240
 82
@Time 1.00 sec
82
@Time 0.000278 hour
ASTM D2240
Tensile Strength at Break 12.1 MPa1750 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain  3.79 MPa
@Strain 50 %
550 psi
@Strain 50 %
Die C, 20 in/min; ASTM D412
 4.27 MPa
@Strain 100 %
620 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 5.45 MPa
@Strain 300 %
790 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 720 %720 %Die C, 20 in/min; ASTM D412
Tear Strength 50.3 kN/m287 pliDie C, 20 in/min; Flow; ASTM D624
Compression Set  25 %
@Temperature 22.8 °C,
Time 79200 sec
25 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 44 %
@Temperature 70.0 °C,
Time 79200 sec
44 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 177 °C320 - 350 °F
Middle Barrel Temperature 182 - 204 °C360 - 400 °F
Front Barrel Temperature 193 - 216 °C380 - 420 °F
Nozzle Temperature 182 - 227 °C360 - 440 °F
Melt Temperature 182 - 227 °C360 - 440 °F
Mold Temperature 26.7 - 48.9 °C80.0 - 120 °F
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 1.27 cm0.150 - 0.500 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0691 / 237182

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.