MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Danquinsa DANCOLL® 245-20F Poly adduct
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCOLL® 245-20F is a high solid poly adduct of low viscosity containing hydroxyl groups which is used for the production of polyethylene bags and film lamination adhesives. This product serves as Tackifier and tack improver in PE bag granular solutions. Furthermore, DANCOLL® 245-20F is added to harder, crystallize PUR-adhesives as a Tackifier.

Application: DANCOLL® 245-20F is supplied in a very soft and elastic version for the bonding of PE-bags. A long lasting inherent tack of the product ensures additional safety in case of long processing cycles. In most cases, DANCOLL® 245-20F is processed together with our poly isocyanate DANCURE® 246-13 in a 2-component way. DANCOLL® 245-20F is used as a modification component for PUR-adhesives when a long open time and a high tack is needed. The amount of the curing agent DANCURE® 246-13 added is approx. 8 to 15% of the total formulation.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³DIN 51.757
Solids Content 73 - 76 %73 - 76 %DIN 53.189
Brookfield Viscosity 2000 - 6000 cP2000 - 6000 cPRVT
 
Thermal PropertiesMetricEnglishComments
Flash Point -3.00 °C26.6 °FDIN 51.755
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Aspectclear and transparent liquid
SolventEthyl acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ021 / 294441

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.