MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Braskem GR105PP 3D Printing Polypropylene Pellets
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: GR105PP is an engineered grade of polypropylene (PP) pellets for 3D printing which provides an excellent balance of mechanical properties, dimensional stability and chemical resistance for use in pellet based 3D printers. This engineered PP grade provides a balance of strength and impact resistance while enabling the production of relatively high strength, watertight, lightweight and chemically resistant parts.

Reported property values are from printed parts; tensile specimens were oriented parallel to the layer direction.

Information provided by Braskem.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 13.0 MPaASTM D638
Tensile Strength, Yield 13.0 MPaASTM D638
Elongation at Break 99 %ASTM D638
Elongation at Yield 5.0 %ASTM D638
Modulus of Elasticity 1.245 GPaASTM D638
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °CASTM D648
Vicat Softening Point 130 °C10 N; ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBRAS690 / 291043

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.