MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C95520, M02 Temper, As Centrifugal Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Centrifugal Cast

Applicable Specifications: As Centrifugal Cast – Castings AMS 4881, Castings SAE J462, Castings SAE J461, Castings AMS B271/B271M; As Continuous Cast – ASTM B505/B505M; As Sand Cast – Castings SAE J461, Castings AMS 4881, Castings SAE J462, Castings ASTM B148; Ingot – ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell >= 262
@Load 0.00306 kg
for Standard
Tensile Strength >= 125 ksifor Standard
Elongation at Break >= 2.0 %for Standard
 
Thermal PropertiesOriginal ValueComments
Annealing Point 925 - 1000 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 600 °FStress Relief
Solution Temperature 1600 - 1700 °F
@Time 120 sec
Water
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 10.5 - 11.5 %
Chromium, Cr <= 0.050 %
Cobalt, Co <= 0.20 %
Copper, Cu >= 74.5 %
Iron, Fe 4.0 - 5.5 %
Lead, Pb <= 0.030 %
Magnesium, Mg <= 1.5 %
Nickel, Ni 4.2 - 6.0 %
Silicon, Si <= 0.15 %
Tin, Sn <= 0.25 %
Zinc, Zn <= 0.30 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC95520x1 / 292628

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.