MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ExxonMobil Paxon™ 7000 Series High Density Polyethylene (HDPE), Crosslinkable
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Crosslinkable (XLPE)

Material Notes: Paxon ™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance.  These resins are ideally suited for applications that require excellent part fill during processing and outstanding finished part performance.  Paxon ™ 7000 series grades are all supplied with long term UV stabilization. 

Availability:  Latin America, North America. 

Applications:  agricultural products, chemical storage tanks, marine fuel tanks, automotive components, large refuse containers, recreational vehicle-fuel tanks.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
ESCR 100% Igepal® >= 1000 hourF0; ASTM D1693
ESCR 10% Igepal® >= 1000 hourF0; ASTM D1693
Degree of Crosslinking 2.5 %ExxonMobil
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2700 psi2.0 in/min; ASTM D638
Elongation at Break 390 %ExxonMobil Method
Elongation at Yield 10 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 110000 psiASTM D790B
Impact Test 64.0 ft-lb
@Thickness 3.17 mm,
Temperature -40.0 °C
ARM
 170 ft-lb
@Thickness 6.35 mm,
Temperature -40.0 °C
ARM
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 136 °Funannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °Funannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Paxon™ 7000 XL Series High Density Polyethylene (HDPE), Crosslinkable
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
ExxonMobil Paxon™ AA48-002 High Density Polyethylene (HDPE), Blow Molding Grade
ExxonMobil HD 7957.04 High Density Polyethylene (HDPE), Film Grade
ExxonMobil HD 6608.19 High Density Polyethylene (HDPE), Injection Molding Grade

PEX98886 / 238268

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.