Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.36 g/cc | 1.36 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 80 | 80 |
| 70 @Temperature 100 °C, Time 252000 sec | 70 @Temperature 212 °F, Time 70.0 hour |
| 70 @Temperature 100 °C, Time 252000 sec | 70 @Temperature 212 °F, Time 70.0 hour |
| 75 @Temperature 23.0 °C, Time 252000 sec | 75 @Temperature 73.4 °F, Time 70.0 hour |
| 85 @Temperature 100 °C, Time 252000 sec | 85 @Temperature 212 °F, Time 70.0 hour |
| 86 @Temperature 100 °C, Time 252000 sec | 86 @Temperature 212 °F, Time 70.0 hour |
Tensile Strength | 8.198 MPa | 1189 psi |
| 7.8779 MPa @Temperature 23.0 °C, Time 252000 sec | 1142.6 psi @Temperature 73.4 °F, Time 70.0 hour |
| 9.85385 MPa @Temperature 100 °C, Time 252000 sec | 1429.18 psi @Temperature 212 °F, Time 70.0 hour |
| 10.575 MPa @Temperature 100 °C, Time 252000 sec | 1533.8 psi @Temperature 212 °F, Time 70.0 hour |
| 10.5752 MPa @Temperature 100 °C, Time 252000 sec | 1533.81 psi @Temperature 212 °F, Time 70.0 hour |
Elongation, Ultimate | 260 % | 260 % |
| 179.92 % @Temperature 100 °C, Time 252000 sec | 179.92 % @Temperature 212 °F, Time 70.0 hour |
| 219.96 % @Temperature 100 °C, Time 252000 sec | 219.96 % @Temperature 212 °F, Time 70.0 hour |
| 230.1 % @Temperature 100 °C, Time 252000 sec | 230.1 % @Temperature 212 °F, Time 70.0 hour |
| 250.12 % @Temperature 23.0 °C, Time 252000 sec | 250.12 % @Temperature 73.4 °F, Time 70.0 hour |
100% Modulus | 4.47 MPa | 649 psi |
Tear Strength | 38.2 kN/m | 218 pli |
Compression Set | 20.6 % @Temperature 100 °C, Time 79200 sec | 20.6 % @Temperature 212 °F, Time 22.0 hour |
| 24.5 % @Temperature 100 °C, Time 79200 sec | 24.5 % @Temperature 212 °F, Time 22.0 hour |
| 31.9 % @Temperature 100 °C, Time 252000 sec | 31.9 % @Temperature 212 °F, Time 70.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | -33.9 °C | -29.0 °F |
Shrinkage | -7.60 % @Temperature 100 °C, Time 252000 sec | -7.60 % @Temperature 212 °F, Time 70.0 hour |
| 2.7 % @Temperature 23.0 °C, Time 252000 sec | 2.7 % @Temperature 73.4 °F, Time 70.0 hour |
| 10.2 % @Temperature 100 °C, Time 252000 sec | 10.2 % @Temperature 212 °F, Time 70.0 hour |
| 12.3 % @Temperature 100 °C, Time 252000 sec | 12.3 % @Temperature 212 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.