MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ASI® Pipe Sealer TORQUE 20RC and TORQUE 20RCHH Anaerobic Methacrylate Ester Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TORQUE 20RC and TORQUE 20RCHH are anaerobic resins that are the best method for retaining, locking, and sealing a wide range of metal parts. Even in the tightest fitting assemblies voids are presents which allows for movement and potential loosening of the parts. TORQUE 20RC and 20RCHH form a tough, durable resin, that fills all these voids, creating a unitized assembly that is completely resistant to shock, vibration, and extremely harsh environmental conditions. These materials cure in the absence of air and in the present of metal. They are suited for retaining cylindrical assemblies providing shock and vibration resistance.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
@Temperature 25.0 °C
uncured
Brookfield Viscosity 8000 cP
@Temperature 20.0 °C
Uncured. Spindle 5- 20 rpm. 20RC
 12000 cP
@Temperature 20.0 °C
Uncured. Spindle 5- 20 rpm. 20RCHV
Storage Temperature 8.00 - 28.0 °Cuncured
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 2000 psiISO 10123
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.0000800 µm/m-°Ccured; ASTM D696
Specific Heat Capacity 0.300 J/g-°Ccured
Thermal Conductivity 0.100 W/m-Kcured; ASTM C177
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °C
Flash Point >= 100 °Cuncured
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 20.0 °C
uncured
 
Descriptive Properties
Chemical ClassMethacrylate Ester
Color / appearanceGreen liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9199 / 233565

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.