MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Daikin FEP Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Daikin FEP film is smooth and high-performing non-stretch film, which is formed by melt extrusion with Daikin FEP material. Daikin FEP film consists of atoms of carbon and fluorine, and has outstanding heat and chemical resistance, nonadhesion, and nonflammability. It also possesses fabricating characteristics, including heat sealing, thermoforming, welding and heat bonding as well as adhesion (surface treatment items).

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.12 - 2.17 g/ccASTM D1505
Particle Size 50 µm
Thickness 50.0 micronsAs Tested
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 352 %ASTM D882
Film Elongation at Yield, MD 388 %ASTM D882
Film Tensile Strength at Break, MD 31.8 MPaASTM D882
Film Tensile Strength at Break, TD 33.5 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.250 W/m-KASTM C177
Melting Point 270 °C
Maximum Service Temperature, Air 200 °CContinuous
Oxygen Index >= 95 %ASTM D2863
Shrinkage, MD 0.80 %
@Temperature 200 °C
ASTM D3595-97
Shrinkage, TD 0.70 %
@Temperature 200 °C
ASTM D3595-97

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
Chemours 340 PFA Perfluoroalkoxy Copolymer
Chemours 100 FEP Fluorinated Ethylene Propylene
AGC Fluon® FEP 100 White Pigmentation
Daikin NEOFLON® NF-0050 FEP Film

PDAIJ9914 / 209985

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.