MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® 3D IND147™ HDT230 High-temperature 3D printing resin
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset

Material Notes: Henkel® Loctite® 3D IND147 High-temperature 3D printing resin for tooling & molding applications. Due to its high stiffness and high-temperature resistance, which withstands temperatures up to 230°C, Henkel Loctite 3D IND147 is a rigid 3D printing resin designed for tooling and molding applications. Loctite 3D IND147 is a high-performance additive manufacturing material developed for digital light processing 3D printing technology (DLP). Its strong mechanical properties deliver high stiffness and toughness while withstanding temperatures up to 230°C. With a smooth surface finish, it can tackle applications like polyurethane and silicone molding. In post-processing, the printed components can be easily painted, sanded, or machined for further finishing.

Applications: agriculture, industrial and manufacturing, injection molding.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccLiquid; ASTM D1475
Viscosity 1905 - 2305 cPLiquid as Supplied; ASTM D7867
 830 cP
@Temperature 65.0 °C
Liquid as Supplied; ASTM D7867
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 29.1 - 32.3 MPaASTM D638
 67.0 MPa
Tensile Strength 75.0 MPa
Elongation at Break 2.0 %
 4.2 - 7.6 %ASTM D638
Modulus of Elasticity 1.013 - 1.287 GPaASTM D638
Tensile Modulus 3192 MPa
Flexural Yield Strength 65.0 - 71.0 MPaASTM D790
Flexural Modulus 1864 - 2242 MPaASTM D790
Resilience 4.0
 40
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 3.00 mm
Post processed. Vertical
 
Descriptive Properties
Caloric Content (MJ/kg)13Post processed. ASTM E1354
ColorBlack
Flammability TestPassASTM E162, Post Processed
Flammability Test, UL94PassAITM@-0002, 6 mm, Post Processed
 PassAITM@-0002, 6 mm, Post Processed
Rate of Smoke GenerationPassPost processed. ASTM E662
Smoke (Gas Components)PassAITM@-0005. 6mm. Post processed.
Smoke DensityPassAITM@-0007, 6 mm, Post Processed
Toxic Gas GenerationCompletePost processed. BSS 7239

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT00_h / 305364

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.