MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

GLS Corporation Versalloy™ XL 9045X-9 TPV Elastomer Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Meets FDA specs
Bonds to PP

General Versalloy® Information: Versalloy® Elastomer Alloys are designed to deliver high performance in demanding applications. Based on TPV technology, these alloys demonstrate the performance properties of a TPV with improved processability and surface quality compared to standard TPVs. A few of the benefits of Versalloy elastomer alloys:

  • Excellent surface quality
  • Easy processing with excellent flow for long, thin flow paths
  • Good compression set
  • High tear strength
  • Highly colorable
  • Low specific gravity

Information provided by GLS Corporation.

All information provided by GLS Corporation. GLS Corporation and PolyOne (now Avient) merged in 2008. This discontinued grade was produced by GLS Corporation and is in MatWeb with the GLS name for historical accuracy.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³
Linear Mold Shrinkage 0.011 - 0.015 cm/cm0.011 - 0.015 in/inASTM D955, modified
Melt Flow 82 g/10 min
@Load 5.00 kg,
Temperature 200 °C
82 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238, modified
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4444
Tensile Strength, Ultimate 2.96 MPa430 psi
Elongation at Break 560 %560 %
100% Modulus 1.17 MPa
@Strain 100 %
170 psi
@Strain 100 %
300% Modulus 1.93 MPa
@Strain 300 %
280 psi
@Strain 300 %
ASTM D412 Die C, modified
Tear Strength 17.5 kN/m100 pli
Compression Set 19 %19 %22 hrs @ 23°C; ASTM D 395B, modified
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZGLSCV51 / 42259

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.