MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemlok® 217 Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Chemlok® 217 adhesive is a one-coat adhesive used to bond nitrile or neoprene elastomers to metals or other substrates during vulcanization of the elastomer. The adhesive provides ample processing latitude and readily adapts to conventional application and molding methods. For maximum protection or when environmental conditions are extremely aggressive, Chemlok 217 adhesive can be used over Chemlok 205 primer.

Features: provides excellent heat and environmental resistance. dries quickly to a hard coating. bonds under a variety of production conditions. requires only a single coat for most applications, reducing labor, solvent usage, inventory and shipping costs. applies easily by spray, dip or brush methods.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.70 - 8.00 lb/gal
Solids Content 23 - 27 %by weight
Brookfield Viscosity 75 - 150 cP
@Temperature 25.0 °C
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point -2.00 °CSeta
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 21.0 - 27.0 °C
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlack liquid
SolventsMethyl Ethyl Ketone (MEK), Xylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9068 / 232457

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.