MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Glyptal 1201 Primer, Sealer, Adhesive, and Protective Finish
Categories: Polymer; Adhesive

Material Notes: Excellent as a general purpose paint. Available in quarts, gallon, 5 gallon pails and drum containers ready for brushing. May be thinned for spray applications. Outstanding resistance to corrosion, moisture, oil, acid, heat, dust, and salt spray. Typical industry uses include:
  • Primer for structural iron and steal
  • General plant maintenance
  • Sealer for concrete floors
  • Primer and finish for motor, generator, and transformer housings
  • Anti-moisture coating on thermostat, water cooler, and truck control parts
  • Sealer for pipe and stud threads and vacuum systems
  • Anti-corrosion protection for winches and other out-door apparatus
  • Electrical insulation for coils and armatures
  • Adhesive for gaskets
  • Coating for interior of hydraulic tanks, and bearing cases

Exhaustive tests conducted at the Glyptal laboratories confirm consistently favorable customer experience with 1201:

  • Meets requirements of MIL-E-22118
  • Flexibility is far superior to competitive re sealers on both backed and air-dried films. 1201 can take rugged impact.
  • Water Resistance is excellent
  • Prolonged Aging doesn't crack 1201's film, leaves no place for destructive agents to get in
  • Fast Drying 1201 is tack-free in about thirty minutes at room temperature, can be baked to a beautiful smooth finish
  • Heat resistance. 1201 has got it, can withstand continuous 135°C temperatures for months.
  • Prolonged Heat. After 3700 hours at 35°C, there is no change in dielectric strength
  • Toughness. High-gloss paints have a tender film. 1201 has a low-gloss finish, designed for great resistance to abrasion.
  • Adhesion. 1201 hangs on, stays where it's put-on metals, ceramic, porcelain, concrete, fibers, and wood
  • Arc Resistance, even with air-dried films, is 480 seconds

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/cc
Solids Content 60 %Weight
Viscosity 325 cP
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 7.50e+7 ohm
@Time 86400 sec
90% RH
Dielectric Strength 1500 V/milDry; ASTM D115-55
 350 V/mil
@Time 86400 sec
In Water
Arc Resistance 480 sec
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 135 °C
Flash Point 72.0 °FClosed Cup
 
Processing PropertiesOriginal ValueComments
Dry Time 0.500 hour1 mil avg. dust-free
Tack-Free Time 2.00 hour1 mil avg. tack-free to handle
 
Descriptive Properties
Chemical ResistanceExcellentOil (transil)
 Fair - low concentrationsAlkali
 GoodWater
 GoodSalt water
 GoodAcid
Solvent SystemXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGLYPT902 / 209741

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.