MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon Diethyleneglycol Mixture (DEG Mix)
Categories: Other Engineering Material

Material Notes: DEG-Mix is a mix of diethylene glycol, monoethylene glycol, triethylene glycol and water. Its main application is as a raw material for grinding aids.

CAS number: 111-46-6 (DEG)

EINECS/ELINCS No.: 203-872-2 (DEG)

Molecular formula: C4H10O3

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
pH 111% solution
Viscosity 20 cPDynamic
Molecular Weight 106.1 g/mol
Vapor Pressure 0.0000280 bar
 
Thermal PropertiesOriginal ValueComments
Melting Point <= -20.0 °C
@Pressure 0.1013 MPa
Boiling Point >= 100 °C
@Pressure 0.1013 MPa
Flash Point 100 - 199 °C
@Pressure 0.1013 MPa
Ignition Temperature >= 100 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 17 - 19 %MOA 208
 
Descriptive Properties
AppearanceDark brown liquid
OdorOdorless
Partition coefficient-1,3N-octanol/water, 20°C, log Pow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY483 / 286006

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.